PF-2LA


特性:

项目 Item 符号Symbol 测定条件 Condition 值 Value 单位 Unit
初始磁导率 Initial permeability μi F:10KHz B<0.25mT 25 2300±25% -
饱和磁通密度 Saturation flux density Bs H:800A/m 25 530 mT
100 410
剩余磁通密度 Remanent flux density Br H→0 (from near saturation) 25 200 mT
100 65
矫顽力 Coercivity Hc B→0 (from near saturation) 25 13 A/m
100 6
居里温度 Curie temperature Tc f:100KHz B<0.25mT   >240
电阻率 Resistivity ρ   25 >4.5 Ωm
密度 Density d     4.8×103 Kg/m3
功耗 Poeer Loss Pcv 100KHz,200mT 25 610 Kw/m3
60 420 Kw/m3
80 - Kw/m3
100 280 Kw/m3
120 380 Kw/m3

 

 

曲线:

材质 Material:PF-2LA

 

【measured with Φ30*19*9 toroid core】